Evaluation And Analysis of The Remaining Life of The Superheater Area Tube Boiler Using the Corrosion Rate Calculation Method

Authors

  • Arrad Ghani Safitra Politeknik Elektronika Negeri Surabaya Author
  • Firman Yunan Saputra Politeknik Elektronika Negeri Surabaya Author

Keywords:

Superheater, Thickness, Corrosion Rate, Remaining Life

Abstract

In coal-fired power plant operations, maintaining the temperature stability of components is crucial for system efficiency and reliability. The superheater serves as a secondary heater for dry steam. One cause of reduced thermal performance is the non-uniform wall thickness of the pipes at various points. This study aims to determine the rate of pipe wall thinning in the superheater at panel 1 as sample area by 2027 using pipe wall thickness data from the 2025 overhaul inspection. The analysis results show that the highest corrosion rate occurs at point D in 2027, with an average of 0.27, resulting in a thinner pipe wall at that point compared to the other pipes. This thickness variation is related to corrosion and erosion caused by fluctuating operating loads.

Downloads

Download data is not yet available.

Downloads

Published

2026-10-30

How to Cite

Evaluation And Analysis of The Remaining Life of The Superheater Area Tube Boiler Using the Corrosion Rate Calculation Method. (2026). Journal of Applied Mechanics, Mechatronics, and Energy Systems, 1(1), 7-11. https://journals.pens.ac.id/jammes/article/view/108